Introduction

Paper machine felts are a valuable material in the paper industry. This practical Q&A covers their classification, selection, installation, correct operation, and solutions to the most common quality problems encountered on the machine.

1. What types of paper machine felts are there?

By application, felts fall into three main types: wet felts, top felts, and dryer felts. On the machine they filter water from the stock and press the wet web from multiple wires tightly together, so wet felts require good water permeability and durability.

2. Felt production process

Weaving → seaming (fitting ends) → base-fabric setting → batt laying → needle punching → setting → finished product.

3. How to select a paper machine felt

Most domestic felt makers now use all-synthetic needle-punched felts, which dewater quickly, absorb little moisture, and need no singeing. For thin paper grades on high-speed machines, a four-ply yarn, plain or broken-twill base fabric with a basis weight of about 700 g/m² (front) is generally used; where light felt marks are required and speed is not too high, 730–750 g/m² is used, and the top felt should be about 50 g/m² heavier. The exact choice depends on the base fabric structure and proportion, the effective power of the vacuum pump, the washing water pressure, the roll diameter, the pressure, and the dryer size.

4. Choosing felt specifications

Follow the principles: longer rather than shorter, wider rather than narrower, and thinner rather than thicker.

5. Notes when changing to a new felt

A felt has a front and back side that differ greatly: the front side has fine, soft fiber, while the back side has coarse, hard fiber and rough setting crystal points.

6. Felt installation

The front side is the sheet-contacting side, and a running-direction arrow is marked on the felt. After installation, first wash with hot water at 50–60°C, adding 5–10% sodium hydroxide or detergent, and run empty for 15–20 minutes. Then run empty (duration depends on actual conditions, generally 2–3 hours) until the felt is fully softened. In the early period, do not set the tension too tight or the speed too high; after two to three days, tension the felt and raise the speed — this benefits felt life.

7. Analysis of problems during felt use

A felt is a filter material serving the paper machine, and a felt is "good" only if it suits the machine. Many apparent felt quality problems are in fact caused by unsuitability to the machine's performance. This requires us to learn more about each customer's machine performance and configuration so we can produce more suitable felts.

8. Handling a felt that widens after use

A felt may widen after some time in use — this is normal. Never tear it by hand; stop the machine, let the felt dry, trim off the excess edge, and then seal the edge with a hot iron.

9. Analysis and treatment of the standard line bending forward or backward

When the standard line bulges toward the running direction, it is mainly caused by excessive crown on the carrier roll; treat by grinding the crown or by increasing carrier-roll pressure (a 400 mm-diameter rubber roll, 45 Shore hardness). When the standard line is concave (bending backward), it is mainly caused by insufficient crown, or by correct crown but excessive pressure. Press roll pressure is generally 30–40 kg/cm².

10. Causes of felt shrinkage

Mainly caused by a loose base fabric structure that is unstable during felt making. Treatment: loosen the tightening rolls and run the felt in a relaxed state. An incorrect standard line is unfavorable to normal felt operation.

11. Felt embossing (printing)

A long-standing difficult problem between mills and felt makers — a headache that is hard to see or grasp. Based on years at a felt maker and in overseas sales, embossing has many causes, and several of the following can trigger it, most commonly in tissue paper: excessive dispersant dosage; insufficient vacuum; too much impurity in the stock; insufficient water pressure; aged carrier-roll rubber; incorrect carrier-roll position; excessive base fabric density, or an unstable base structure with uneven density; excessive density at the seam; and felt weight too high with improper coarse/fine fiber blending. This calls for good equipment performance and for sales staff to understand both machine and felt performance, so the felt and machine can find common ground and serve the machine effectively.

12. Finding and treating embossing points

When embossing is caused by a blockage, find the point accurately as follows: first pull off the stock, slow the machine, and keep water and vacuum running; after the felt is clean, stop the water and run vacuum a few more turns, then stop; once the felt dries, the embossing point appears white. Pick out the blockage with a needle. On the back side of the point, cut a few weft yarns (three to five), and the treatment is complete.

13. Why a new felt picks up stock, and how to treat it

New-felt stock pickup is usually caused by a rough surface or an uneven felt surface; brushing with a brass brush can help somewhat. For a felt that has been used a while, it is caused by fiber being too long — singe it with a torch.

14. Why the felt does not carry stock, and how to treat it

Caused by a felt surface that is too smooth, insufficient crown on the press roll, or excessive sheet moisture.

15. Causes of holes in the felt

Inadvertent mechanical damage by the operator, or — where the surface is intact but the base fabric has a hole — stock dropped onto the felt and broke the warp and weft yarns under pressure.

16. Can the back side be used when a felt performs poorly?

It depends on the felt structure. Felts that can be reversed: plain-weave felts and ordinary felts. Broken-twill felts cannot be reversed. In principle, a reversible felt should not have overly fine front-side fiber, otherwise impurities easily enter and cause embossing.

17. Why no paper is produced when speed is increased

If the machine runs paper below 100 m/min but only pulp residue comes off the dryer when speed is raised, the cause is insufficient height of the preheating roll; raising it slightly solves the problem.

18. Paper not dry at increased speed

Two cases: the whole width is not dry, or only the edges are not dry. If the whole width is not dry, the felt is too thick or the dryer is too small.

19. Felt service life too short

Look at how the felt came off the machine: poor dewatering at end of life, poor sheet surface, or worn out. This can be seen from the removed felt. If the suction-box cover is uneven, the material is coarse, or the holes are too large, felt friction increases and life is shortened.

20. Small holes on the sheet surface

One cause is sand holes around the felt circumference from weft yarns appearing during needling; another is weft yarns at the seam. If irregular sand holes appear, the causes may be: (1) sand in the stock; (2) stock that sprayed onto the felt during wire washing; (3) pitting on the press roll.

21. Installation and pressure of the felt washing showers

Moving showers are better than fixed ones, and fan-shaped nozzles are better than cylindrical ones; water pressure is generally 3–5 kg. Installation matters: the back-side pressure shower is placed in front and the front-side pressure shower behind; the back-side pressure should be higher and the front-side lower; the back sprays at 90° and the front at 35–45° downward. When an embossed felt is cleaned with high-pressure water, never spray the front side — it will raise the nap; use a water gun on the back side only.

22. Vacuum level values

Generally keep vacuum at 150–200 mmHg (ordinary felt 100–150 mmHg; endless base fabric 200–250 mmHg). Many mills neglect felt maintenance to raise output, but the quality of felt maintenance directly affects its use and life.

23. Correct method of use

A new felt should run slowly at 70–80 m/min for two to three hours, then be raised to 90–100 m/min after 24 hours, to 100–130 m/min after 36 hours, and then to full speed. Clean once a week after the first week of use. The felt conditioner (beater) should only be used in the late stage of felt life. Before washing, understand the felt material: polyester resists acid but not alkali, while nylon resists alkali but not acid. Mix the detergent accordingly. If acid washing is necessary, strictly control it at 3–5%; nylon felt must not be acid-washed, because acid melts it and leaves the surface gelatinous and unusable. Rinse thoroughly with fresh water after washing, and residual acid can be neutralized with alkali.

24. Analysis and treatment of standard-line deviation or forward/backward bending

Standard-line deviation can result from: (1) the two edges of the felt being unequal in length; (2) machine roll axes not being parallel, causing uneven felt tension; (3) uneven watering after a shutdown and restart, causing inconsistent shrinkage. All of these can deform, deviate, or fold the standard line.